ASTM E3047 – Standard Test Method for Analysis of Nickel Alloys by Spark Atomic Emission Spectrometry
1.1 This method describes the spark atomic emission spectrometric (Spark-AES) analysis of nickel alloys, such as those specified by committee B02, having chemical compositions within the following limits:
|
Element |
Application Range (Mass Fraction, %) |
|
Aluminum |
0.005-6.00 |
|
Boron |
0.001-0.10 |
|
Carbon |
0.005-0.15 |
|
Chromium |
0.01-33.00 |
|
Copper |
0.01-35.00 |
|
Cobalt |
0.01-25.00 |
|
Iron |
0.05-55.00 |
|
Magnesium |
0.001-0.020 |
|
Manganese |
0.01-1.00 |
|
Molybdenum |
0.01-35.00 |
|
Niobium |
0.01-6.0 |
|
Nickel |
25.00-100.0 |
|
Phosphorous |
0.001-0.025 |
|
Silicon |
0.01-1.50 |
|
Sulfur |
0.0001-0.01 |
|
Titanium |
0.0001-6.0 |
|
Tantalum |
0.01-0.15 |
|
Tin |
0.001-0.020 |
|
Tungsten |
0.01-5.0 |
|
Vanadium |
0.0005-1.0 |
|
Zirconium |
0.01-0.10 |